Over-Spray Roughness

* An example of this type of paint challenge, but not necessarily the only representation.
PAINT ISSUE:
how to remove overspray from paint -OR- overspray on car paint -OR- rough texture after painting car
PREVENTION:
- Agitate and mix metallic paint thoroughly before and during use; use mechanical shaker if possible.
- Avoid heavy or wet coats that allow flakes to settle.
- Do not allow basecoat to dry too long before clear.
- Spray with even overlap, correct gun distance, and moderate air pressure.
- Use only recommended reducer and spray technique for metallics.
TO REPAIR:
- Blend into adjacent panels if needed for uniform metallic effect.
- Reapply basecoat with proper mixing and spraying technique.
- Sand out blotchy or dropout areas with 1500 grit.